Enhancing Lithium Battery Safety in Transportation

A conversation with Carlos F. Lopez, P.E. of Stress Engineering Services... In the rapidly evolving landscape of energy storage, lithium-ion batteries play a pivotal role. However, the safety of these batteries during transportation remains a significant concern due to the risk of...

read More....
0
15
Oct 2024

Additively Manufactured Components Testing: Our Comprehensive Process for Full-Scale Validation

By: Patrick L. Boster, PEAt Stress Engineering Services, we recognize that transitioning from concept to solution in additively manufactured parts encompasses numerous complex challenges. This article describes our full-scale testing process, specifically engineered to overcome these...

read More....
0
14
Aug 2024

Carbon Capture and Sequestration: Developments in Injection Well Metallurgy

By: Adam C. Rowe, P. E.Carbon Capture and Sequestration (CCS) is recognized as a crucial carbon management technology, and projects to capture, transport, and store CO2 are continuing to garner significant attention. While construction of CCS facilities is in many ways similar to...

read More....
0
02
Aug 2024

The Importance and Benefit of Full-Scale Testing for Additively Manufactured Parts

By: Patrick L. Boster, PENavigating the challenges of additive manufacturing requires more than innovative design; it demands rigorous testing to ensure operational viability. Full-scale testing bridges the gap between prototype and real-world application, providing a comprehensive...

read More....
0
11
Jul 2024

Laser Internal Inspection: Revolutionizing Tubing Durability in Shale Operations

By: Jason WaliguraAs the demand for more durable and longer-lasting production tubing in shale operations increases, Stress Engineering Services (SES) is leading the way with groundbreaking solutions. A prime example of such innovation is the use of boronized production tubing in...

read More....
07
Jun 2024

Case Study: Oil Refinery Operator + Lincoln Electric Additive Manufacturing

Accelerating Routine Maintenance Timelines with WAAM Parts from Lincoln Electric Stress Engineering Services (SES), a leader in qualification and testing, partners with industry leaders across aerospace, defense, medical, energy, nuclear, and automotive sectors. When a domestic...

read More....
02
May 2024

Unlocking the Mystery of Hard Spots on Vintage Pipes

By: Sri Chimbli, PE, AWS CWEng/CWIOver the years, vintage pipes have often been subject to unexpected ruptures, a phenomenon attributed to the presence of 'hard spots'. These are areas of heightened hardness on the outside surface, exceeding 327 HB (35 HRC). The ability to accurately...

read More....
0
27
Mar 2024

Ensuring Employee Safety: Navigating Hot Weather Hazards in the Workplace

As the sun blazes down during the scorching summer months, the importance of prioritizing the safety and well-being of your staff in hot weather conditions cannot be overstated. Rising temperatures can pose significant risks to employees, leading to heat-related illnesses and...

read More....
0
24
Aug 2023

Accelerating the Aging Process: Pressure Cycle Testing to Improve Product Design, Development, and Qualification

By: Matthew W. Sanders, PETesting is critical in developing and manufacturing high-quality and high-performance products, since it can provide valuable insights into a product's strengths and weaknesses. This allows manufacturers to make informed decisions about design, materials,...

read More....
13
Feb 2023
Close

Contact Us

If you would like more information on Stress Engineering Services, please call us at 281.955.2900, or complete the following form and one of our representatives contact you shortly. For a complete listing of contact information, visit our Locations page.

"*" indicates required fields

This field is for validation purposes and should be left unchanged.